Property | Method of testing | Value |
Melt temp | 160-165° C | |
Max use temp | 90° C | |
Vicat softening point | ISO 306/A | 152° C |
HDT | ISO 75/B | 100° C |
Flexural modulus | ISO 178 | >1350 N/mm2 |
Tensile strength @ yield | ISO R 527 | 27 N/mm2 |
Elongation @ yield | ISO R 527 | 8% |
Density | ISO 1183 | 0.9G/cm3 |
Izod impact strength 23°C | ISO 180 | 40 kJ/m |
Izod impact strength -20°C | ISO 180 | 8 kJ/m |
Rockwell hardness | ISO 868 | 68 D scale |
Average compression strength of 8mm – 1800 gr/m2 = 86 Ton/m2 = 0,86 Mpa. |